Trial Purpose:

To evaluate two products for marble immersion.

Date Run:

08/08/2005

Experiment Procedure:

Several marble chips of similar size and shape were weighed to determine the baseline weight of each piece. The selected chips were then immersed in the two supplied products at vendor recommended dilutions and allowed to soak for 18 hours. The marble chips were removed from the products and rinsed in a tap water spray at 120 F for 3 minutes to remove loose material from the chips. Then the chips were dried for 15 minutes using a Master Appliance Heat gun at 300 F. When the chips cooled to room temperature, final weights were recorded to determine weight loss, if any. Observations were made and photographs were taken after the initial immersion of the chips into solutions (5 minutes), at 60 minutes and then following the overnight immersion.

Trial Results:

Neither of the two products changed the weight of the marble chips to any significant level. Both dissolved less than 0.2% The table lists the initial and final weights as well as the removal percentages. Photographs are also included for the three time intervals and for the marble chips after soaking.

Product Initial wt Final wt % Wt loss
Super H2O2 6.3208 6.3165 0.07
  10.1586 10.1477 0.11
  28.0580 28.0545 0.01
  27.3926 27.3743 0.07
H2Orange2 7.2469 7.2188 0.39
  16.2702 16.2590 0.07
  26.6182 26.5973 0.08
  31.7948 31.7579 0.12

Success Rating:

A cleanliness study, addressing only various analytical techniques.

Conclusion:

Both products did not dissolve the marble.